XRF oxide assay
Celestine
Pakistan sample, fine cut. Oxide concentrations with uncertainty and peak / background counts.
- SrO
- 49.274%
- SO₃
- 42.40%
Method · XRF oxide
| Element | Result |
|---|---|
| SrO | 49.274% |
| SO₃ | 42.40% |
| SiO₂ | 4.43% |
| Al₂O₃ | 1.300% |
| TiO₂ | 0.496% |
| MgO | 0.469% |
| CaO | 0.380% |
| BaO | 0.294% |
| K₂O | 0.1481% |
| CuO | 0.0399% |
| Fe₂O₃ | 0.0385% |
| ZnO | 0.012% |
| MnO | 0.011% |
- Sample ident
- Pakistan Sample fine Cut
- Report no.
- Fine cut
- Sampling
- Sample as provided (fine cut)
XRF oxide printout for a Pakistan fine-cut sample. Table lists detected oxides. Values printed in brackets on the sheet (near the detection floor) and fixed light elements (B, Be, Li, CO₂, H₂O) are omitted. Findings relate to the sample as provided.